Diameters / Packaging
Diameters |
22.7 KG BAG |
---|---|
Flux | ED032765 |
DETAILS
Active flux for limited pass welding. Manganese alloying and carbon reducing flux designed to provide superior crack resistance. Slow freezing slag for a wide, flat weld. Excellent resistance to cracking in single pass applications
Features
- Manganese alloying and carbon reducing flux designed to provide superior crack resistance
- Slow freezing slag for a wide, flat weld
- Excellent resistance to cracking in single pass applications
- Actual (Type 3.1) certificates for each lot of flux showing chemical composition, particle size and moisture level are available in the certificate center of lincolnelectric.com
Typical Applications
- Single pass welding of mild steel
- Large fillets with constant current power sources
Special Features
- Basicity Index: 0.8 Density: 1.2 g/cm3
Service Information
You May Also Need
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
MECHANICAL PROPERTIES
Wire | Classification | Postweld Heat Treatment |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
Charpy V-Notch
J (ft-lbs) @ -20°C (0°F) |
Charpy V-Notch
J (ft-lbs) @ -30°C (-20°F) |
---|---|---|---|---|---|---|---|
Lincolnweld® Emergence® 70 | F8TA0-EA1 | As-welded | 510 (74) | 610 (89) | 26 | 34 (25) | |
Lincolnweld® L-50® | F7A2-EM13K-H8 | As-welded | 430 (62) | 560 (81) | 27 | 60 (44) | |
Lincolnweld® L-60 | F7A2-EL12-H8 | As-welded | 440 (64) | 560 (81) | 27 | 70 (52) | |
Lincolnweld® L-61® | F7A2-EM12K-H4 | As-welded | 420 (61) | 540 (78) | 28 | 65 (48) | |
Lincolnweld® L-70 | F9A0-EA1-G | As-welded | 550 (80) | 650 (94) | 25 | 52 (38) | |
Lincolnweld® LA-75 | F8A0-ENi1K-G-H8 | As-welded | 480 (69) | 610 (88) | 27 | 72 (53) |
DEPOSIT COMPOSITION
Wire | Classification | %C | %Cr | %Cu | %Mn | %Mo | %Ni | %P | %S | %Si |
Diffusible Hydrogen
mL/100g Weld Metal |
---|---|---|---|---|---|---|---|---|---|---|---|
Lincolnweld® L-50® | F7A2-EM13K-H8 | 0.03 | 0.08 | 1.93 | 0.017 | 0.080 | 1.02 | 3 | |||
Lincolnweld® L-60 | F7A2-EL12-H8 | 0.04 | 0.08 | 1.70 | 0.020 | 0.007 | 0.78 | 3 | |||
Lincolnweld® L-61® | F7A2-EM12K-H4 | 0.05 | 0.06 | 1.78 | 0.020 | 0.008 | 0.89 | 3 | |||
Lincolnweld® L-70 | F9A0-EA1-G | 0.04 | 0.16 | 1.83 | 0.026 | 0.009 | 0.84 | ||||
Lincolnweld® LA-75 | F8A0-ENi1K-G-H8 | 0.05 | 0.04 | 0.11 | 1.83 | 0.00 | 0.75 | 0.017 | 0.006 | 1.04 | 4 |
FLUX COMPOSITION
Classification | %Al2O3 | %CaF2 | %FeO | %MgO | %MnO | %Na2O | %SiO2 | %TiO2 | %Metal Alloys |
---|---|---|---|---|---|---|---|---|---|
Typical Result | 2 | 5 | 3 | 21 | 21 | 3 | 44 | 2 | 6 max. |