Diameters / Packaging
Diameters |
7.0KG SPOOL |
---|---|
1.0MM | 85ASMAS1210 |
1.2MM | 85ASMAS1212 |
DETAILS
In wide-mouth welding applications, it is recommended to apply a 150-200 ° C preheat to the workpiece before welding and to clean the welding area thoroughly. Since the welding bath has a high fluidity, it should be welded in a horizontal position.