Diameters / Packaging
Diameters |
10 lb (4.5 kg) Easy Open Can |
---|---|
5/32 x 14 in (4.0 x 350 mm) | EL112LFE156634 |
DETAILS
TECH-ROD® 112LFe product is designed to have less than 1% Iron (Fe) for overlay applications where low iron is required, typically achieves Fe levels of 1% or less in the weld deposit.
Features
- A low iron version of the standard Tech-Rod® 112 covered electrode which is used to weld nickel-chromium-molybdenum alloys
- The product is designed to have less than 1% Iron (Fe) for overlay applications where low iron is required
- Product typically achieves Fe levels of 1% or less in a weld deposit
- Q2 Lot® - certificates showing actual deposit composition available online
Typical Applications
- Used extensively in overlay cladding where a similar chemical composition is required on the clad side
- Dissimilar joints between nickel-chromium molybdenum alloys to stainless steels, carbon or low alloys steels
- Welding alloy 625
Welding Positions
- Polarity DC+
Shielding Gas
- N/A
Service Information
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.11 | ENiCrMo-3 |
MECHANICAL PROPERTIES
Classification |
Tensile Strength
MPa (ksi) |
Elongation
% |
---|---|---|
ENiCrMo-3 Requirement | 760 (110) min. | 30 min. |
Typical Result, As-welded | 770 (112) | 43 |
DEPOSIT COMPOSITION
Classification | %C | %Cr | %Cu | %Fe | %Mn | %Mo | %P | %S | %Si | %Nb+Ta | %Ni+Co |
---|---|---|---|---|---|---|---|---|---|---|---|
ENiCrMo-3 Requirement | 0.10 max. | 20.0 - 23.0 | 0.50 max. | 7.0 max. | 1.0 max. | 8.0 - 10.0 | 0.03 max. | 0.02 max. | 0.75 max. | 3.15 - 4.15 | 55.0 min. |
Typical Result | 0.04 | 22.6 | 0.00 | 0.8 | 0.5 | 8.7 | 0.01 | 0.00 | 0.30 | 3.76 | 62.8 |
TYPICAL OPERATING PROCEDURES
Diameter |
Current
Amps |
---|---|
1/8" (3.2 mm) | 80-110 |
5/32" (4.0 mm) | 110-140 |
3/16" (4.8 mm) | 110-160 |