DETAILS
LINCOLN® ER308/308L provides a balanced chromium and nickel levels provide enough ferrite in the weld for high resistance to hot cracking, dual classification ensures the maximum carbon content is 0.03% and ink jet printing identification on entire length of electrode.
Features
- Balanced chromium and nickel levels provide enough ferrite in the weld for high resistance to hot cracking
- Dual classification ensures the maximum carbon content is 0.03%
- 0.03% carbon content increases resistance to intergranular corrosion
- Ink jet printing identification on entire length of electrode
Disclaimers
Service Information
Documentation
You May Also Need
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
See test result disclaimer
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.9 | ER308, ER308L |
ABS | AWS A5.9 | ER308, ER308L |
CWB | CSA W48 | ER308, ER308L |
MIL | MIL-E-19933E AMD1 | MIL-308, MIL-308L |
WIRE COMPOSITION
Classification | %C | %Cr | %Cu | %Mn | %Mo | %N | %Nb | %Ni | %P | %S | %Si | %Ti | Ferrite Number (Delong ©) | Ferrite Number (WRC-1992 ©) |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
ER308 Requirement | 0.08 max. | 19.5 - 22.0 | 0.75 max. | 1.0 - 2.5 | 0.75 max. | 9.0 - 11.0 | 0.03 max. | 0.03 max. | 0.30 - 0.65 | |||||
ER308L Requirement | 0.03 max. | 19.5 - 22.0 | 0.75 max. | 1.0 - 2.5 | 0.75 max. | 9.0 - 11.0 | 0.03 max. | 0.03 max. | 0.30 - 0.65 | |||||
Typical Result | 0.01-0.02 | 19.7-20.3 | 0.04-0.33 | 1.2-1.9 | 0.06-0.15 | 0.02-0.06 | 0.02 max. | 10.1-10.4 | 0.02 | 0.01 max. | 0.34-0.57 | 0.00 max. | 10-16 | 10-14 |