Blue Max Stainless Wire

Diameters / Packaging

Diameters
33 lb (15 kg) Steel Spool
0.035 in (0.9 mm) MG413035667
0.045 in (1.1 mm) MG413045667
1/16 in (1.6 mm) MG413062667

Techalloy® 413

MIG (GMAW)

CLASSIFICATIONS:
AWS ERCrNi

TECHALLOY® 413 Metal Inert Gas Wire designed for MIG and TIG of 70/30, 80/20 and 90/10 copper-nickel alloys applications.

DETAILS

TECHALLOY® 413 ideal for MIG overlay on steel after a first layer with Nickel 208, preheating is generally not required for this product.

Features

  • This filler metal can be used for MIG overlay on steel after a first layer with Nickel 208
  • Preheating is generally not required for this product
  • Q2 Lot® -Certificate showing actual wire composition available online

Typical Applications

  • Used for MIG and TIG of 70/30, 80/20 and 90/10 copper-nickel alloys
  • Maintenance and Repair
  • Overlay after first layer with Nickel 208

Welding Positions

  • All

Shielding Gas

  • MIG 75% Argon / 25% Helium

Disclaimers

Warning -

Cancer and Reproductive Harm -

www.P65Warnings.ca.gov

BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page

See test result disclaimer

CONFORMANCE

CONFORMANCES SPECIFICATION CLASSIFICATION
AWS AWS A5.7 ERCuNi
CWB AWS A5.7 ERCuNi
MIL MIL-E-21562E EN67

WIRE COMPOSITION

Classification %Fe %Mn %P %Pb %S %Si %Ti %Cu+Ag %Ni+Co
ERCuNi Requirement 0.40 - 0.75 1.0 max. 0.02 max. 0.02 max. 0.01 max. 0.25 max. 0.20 - 0.50 Remainder 29.0 - 32.0
Typical Result 0.55 0.6 0.00 max. 0.00 max. 0.00 max. 0.03 0.34 68 30.7

TYPICAL OPERATING PROCEDURES

Diameter Shielding Gas Polarity Voltage
volts
Approx. Current
amps
.035" (0.9 mm) 75% Ar, 25% He DC+ 25-29 150-190
.045" (1.1 mm) 75% Ar, 25% He DC+ 25-28 180-240
1/16" (1.6 mm) 75% Ar, 25% CO2 DC+ 29-33 200-250