UltraCore flux-cored wire
UltraCore flux-cored wire

Diameters / Packaging

Diameters
33 lb Spool
0.045 in (1.1 mm) ED037122
1/16 in (1.6 mm) ED037123

UltraCore® FC 316L

Flux-Cored Gas-Shielded (FCAW-G) | ED037122

AWS:
AWS E316T0-1
E316T0-4
E316LT0-1
E316LT0-4

Smooth arc action with minimal spatter reduces post-weld cleaning

DETAILS

ULTRACORE® 316L produces stabilized nitrogen titanium and niobium chemical composition ideal for polished weld bead appearance and smooth arc action with minimal spatter reduces post-weld cleaning during welding operations.

Features

  • Precision layer wound winding delivers steady spool payoff and more consistent feeding
  • Smooth arc action with minimal spatter reduces post-weld cleaning
  • Polished weld bead appearance reduces post-weld brushing
  • Vacuum sealed foil packaging to keep moisture out

Disclaimers

Warning -

Cancer and Reproductive Harm -

www.P65Warnings.ca.gov

You May Also Need

BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page

See test result disclaimer

CONFORMANCE

CONFORMANCES SPECIFICATION CLASSIFICATION
AWS AWS A5.22 E316LT0-1, E316LT0-4
ABS AWS A5.22 E316LT0-1, E316LT0-4
CWB AWS A5.22 E316LT0-1, E316LT0-4

MECHANICAL PROPERTIES

Classification Shielding Gas Tensile Strength
MPa (ksi)
Elongation
%
Longitudinal Face Bend
E316LT0-1 Requirement 100% CO2 480 (70) min. 30 min. No opening in excess of 1/8 inch
E316LT0-4 Requirement 75-80% Ar, balance CO2 480 (70) min. 30 min. No opening in excess of 1/8 inch
Typical Result, As-welded 100% CO2 550 (80) 46 Passed
Typical Result, As-welded 75% Ar, 25% CO2 540 (79) 52 Passed

DEPOSIT COMPOSITION

Classification Shielding Gas %C %Cr %Cu %Mn %Mo %N %Ni %P %S %Si Ferrite Number (per AWS A4.2)
E316LT0-1 Requirement 100% CO2 0.04 max. 17.0 - 20.0 0.75 max. 0.5 - 2.5 2.0 - 3.0 Info. Only 11.0 - 14.0 0.04 max. 0.03 max. 1.0 max. Info. Only
E316LT0-4 Requirement 75-80% Ar, balance CO2 0.04 max. 17.0 - 20.0 0.75 max. 0.5 - 2.5 2.0 - 3.0 Info. Only 11.0 - 14.0 0.04 max. 0.03 max. 1.0 max. Info. Only
Typical Result 100% CO2 0.04 17.9 0.07 1.2 2.6 0.03 12.4 0.02 0.01 0.7 7
Typical Result 75% Ar, 25% CO2 0.03 18.1 0.07 1.4 2.5 0.03 12.2 0.02 0.01 0.8 8

TYPICAL OPERATING PROCEDURES

Diameter Shielding Gas Polarity CTWD
mm (in.)⁽¹⁾
Wire Feed Speed
m/min (in/min)
Voltage
volts
Approx. Current
amps
Melt-off Rate
kg/hr (lb/hr)
Deposition Rate
kg/hr (lb/hr)
Efficiency
%
0.045 in (1.1 mm) 75% Ar / 25% CO2 DC+ 19 (3/4) 5.3 (210) 22-24 130 2.2 (4.8) 1.9 (4.1) 85.4
0.045 in (1.1 mm) 75% Ar / 25% CO2 DC+ 19 (3/4) 8.9 (350) 24-26 175 3.7 (8.2) 3.2 (7.0) 85.3
0.045 in (1.1 mm) 75% Ar / 25% CO2 DC+ 19 (3/4) 11.4 (450) 26-28 210 4.6 (10.1) 4.1 (9.0) 89.1
1/16 in (1.6 mm) 75% Ar / 25% CO2 DC+ 25 (1) 3.6 (140) 23-25 155 2.7 (5.9) 2.3 (5.0) 84.7
1/16 in (1.6 mm) 75% Ar / 25% CO2 DC+ 25 (1) 6.4 (250) 25-27 230 4.8 (10.6) 4.3 (9.4) 88.6
1/16 in (1.6 mm) 75% Ar / 25% CO2 DC+ 25 (1) 8.1 (320) 26-28 280 6.2 (13.6) 5.5 (12.1) 88.9

NOTES

Note
⁽¹⁾ To estimate ESO, subtract 1/4 in. (6.0 mm) from CTWD.