Diameters / Packaging
Diameters |
8 lb (3.6 kg) Easy Open Can |
---|---|
1/8 x 12 in (3.2 x 300 mm) | ED033099 |
DETAILS
EXCALIBUR® 309/309L-15 provides a low carbon weld deposit to help eliminate carbide precipitation. The fast freezing flux coating is great for vertical down welding.
Features
- Fast freezing slag is great for vertical down welding
- Designed with low carbon levels to help eliminate carbide precipitation
- Q2 Lot® - Certificate showing actual deposit composition and ferrite number (FN) by ferrite scope available online
Service Information
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.4 | E309-15, E309L-15 |
ABS | AWS A5.4 | E309-15, E309L-15 |
MECHANICAL PROPERTIES
Classification |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
---|---|---|---|
E309-15 Requirement | 550 (80) min. | 30 min. | |
E309L-15 Requirement | 520 (75) min. | 30 min. | |
Typical Result, As-welded | 470-500 (68-72) | 620-640 (90-93) | 31-38 |
DEPOSIT COMPOSITION
Classification | %Bi | %C | %Cr | %Cu | %Mn | %Mo | %N | %Ni | %P | %S | %Si | Ferrite Number (per AWS A4.2) |
---|---|---|---|---|---|---|---|---|---|---|---|---|
E309-15 Requirement | 0.15 max. | 22.0 - 25.0 | 0.75 max. | 0.5 - 2.5 | 0.75 max. | 12.0 - 14.0 | 0.04 max. | 0.03 max. | 1.00 max. | |||
E309L-15 Requirement | 0.04 max. | 22.0 - 25.0 | 0.75 max. | 0.5 - 2.5 | 0.75 max. | 12.0 - 14.0 | 0.04 max. | 0.03 max. | 1.00 max. | |||
Typical Result | 0.001-0.002 | 0.02-0.03 | 22.6-23.7 | 0.03-0.10 | 0.7-1.0 | 0.02-0.21 | 0.09-0.15 | 13.3-13.6 | 0.02-0.03 | 0.01-0.02 | 0.94-1.00 | 2-10 |
TYPICAL OPERATING PROCEDURES
Diameter | Polarity⁽¹⁾ |
Current
Amps |
---|---|---|
3/32 in (2.4 mm) | DC+ | 60-70 |
1/8 in (3.2 mm) | DC+ | 90-100 |
NOTES
Note |
---|
⁽¹⁾ Preferred polarity is listed first. |