DETAILS
Low alloy stick electrode designed for Chromium-molybdenum and other low alloy steels, including AISI 4130, 4140, 8630 and ASTM A182 and A336 Grades F22
Features
- Q2 Lot® - Lot Controlled Chemistry and Mechanical Properties
- Premium arc performance
- Easy strike
- Easy slag removal
Service Information
You May Also Need
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Search page
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.5 | E10018-D2 H4R |
ABS | ABS - Part 2 | 3YQ620 H5 |
CWB | CWB AWS A5.5 | E6918-D2 (E10018-D2-H4R) |
DNV-GL | DNV - 2.9 | 3 Y62H5 |
LR | LR - Chapter 11 | 3Y62M H5 |
MECHANICAL PROPERTIES
Classification |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
Charpy V-Notch
J (ft-lbs) @ -50°C (-60°F) |
Hardness Rockwell B |
---|---|---|---|---|---|
E10018-D2 H4R Requirement | 600 (87) min. | 690 (100) min. | 16 min. | ||
Typical Result, 1 hour @ 620°C (1150°F) | 670-850 (98-123) | 760-920 (110-134) | 17-25 | 27-70 (20-52) | 98-105 |
DEPOSIT COMPOSITION
Classification | %C | %Mn | %Mo | %Ni | %P | %S | %Si |
Diffusible Hydrogen
mL/100g Weld Metal |
1800F H2O - As received | 1800F H2O - After 9 hrs at 80F/80%RH |
---|---|---|---|---|---|---|---|---|---|---|
E10018-D2 H4R Requirement | 0.15 max. | 1.65 - 2.00 | 0.25 - 0.45 | 0.90 max. | 0.03 max. | 0.03 max. | 0.80 max. | 4 max. | 0.15 max. | 0.4 max. |
Typical Result | 0.08-0.14 | 1.82-1.98 | 0.36-0.41 | 0.69-0.83 | 0.01-0.02 | 0.01 | 0.38-0.49 | 2-4 | 0.05-0.13 | 0.1-0.4 |
TYPICAL OPERATING PROCEDURES
Diameter | Polarity |
Current
Amps |
---|---|---|
3/32 in (2.4 mm) | DC+ | 60-110 |
3/32 in (2.4 mm) | AC | 65-120 |
1/8 in (3.2 mm) | DC+ | 85-160 |
1/8 in (3.2 mm) | AC | 90-170 |
5/32 in (4.0 mm) | DC+ | 110-210 |
5/32 in (4.0 mm) | AC | 115-220 |