Diámetros/embalaje
Diámetros |
Tubo 5 KG |
---|---|
2.4 mm | T9CRMO-24 |
DETALLES
Varilla TIG para aleación martensítica 9%Cr-1%Mo para servicio a temperaturas elevadas de hasta 600°C
Características
- B8 alloyed steel: 9% chromium, 1% molybdenum martensitic alloy for elevated temperature service up to 600°C (1112°F)
- Designed for high strength and improved corrosion resistance in superheated steam, hot hydrogen gas and high sulphur crude oils where higher performance than 5% chromium, 0.5% molybdenum steels is required
- Disponible en tubo de PE
Información de mantenimiento
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. Página de búsqueda de HDS
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.28 | ER80S-B8 |
MECHANICAL PROPERTIES
Classification | Postweld Heat Treatment | Shielding Gas | Polarity |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
---|---|---|---|---|---|---|
ER80S-B8 Requirement | 100% Ar | DC- | 470 (68) min. | 550 (80) min. | 17 min. | |
Typical Result, Stress relieved | 1 hour @ 745°C (1375°F) | 100% Ar | DC- | 600 (88) | 720 (104) | 23 |
WIRE COMPOSITION
Classification | %C | %Cr | %Mn | %Mo | %Ni | %P | %S | %Si | %Total Cu |
---|---|---|---|---|---|---|---|---|---|
ER80S-B8 Requirement | 0.10 max. | 8.00 - 10.50 | 0.40 - 0.70 | 0.80 - 1.20 | 0.50 max. | 0.025 max. | 0.025 max. | 0.50 max. | 0.35 max. |
Typical Result | 0.09 | 8.58 | 0.51 | 0.94 | 0.08 | 0.016 | 0.002 | 0.42 | 0.05 |