Techalloy Stainless TIG Cut Length Consumables

Diámetros / Embalaje

Diámetros
mm
10 lb (4.5 kg) Plastic Tube
3/32 in (2.4 mm) TG99093638

Techalloy® 99 TIG

Soldadura de Arco Eléctrico con Tungsteno y Gas (GTAW) | TG99093638

CLASIFICACIONES:
ERNi-CI

TECHALLOY® 99 Tungsten Inert Gas Rod designed for welding alloys 718, 706 and X-750 applications.

Detalles

TECHALLOY® 99 is ideal for welding high strength aircraft components and liquid rocket components involving cryogenic temperatures, can be age hardened to higher strengths deposit.

Características

  • Welds produced are generally more machinable than a Tech-Rod® 55 deposit
  • A preheat and inter-pass temperature of not less than 350°F (175°C) is required during welding on cast iron to minimize the potential for cracks
  • Q2 Lot® - certificates showing actual wire composition available online

Servicio de información

ANTES DE USARLO, LEA Y COMPRENDA LA HOJA DE DATOS DE SEGURIDAD (SDS) DE ESTE PRODUCTO Y LA INFORMACIÓN ESPECÍFICA IMPRESA EN EL ENVASE DEL PRODUCTO. Página de Búsqueda SDS

Ver los resultados de la prueba de limitación de responsabilidad

CONFORMANCE

CONFORMANCES SPECIFICATION CLASSIFICATION
AWS AWS A5.15 ERNi-CI

WIRE COMPOSITION

Classification %C %Cu %Fe %Mn %S %Si %Ni+Co
ERNi-CI Requirement 1.0 max. 4.0 max. 4.0 max. 2.5 max. 0.03 max. 0.75 max. 90 min.
Typical Result 0.0 max. 0.01 max. 0.1 0.01 max. 0.003 max. 0.15 100