Developed for 5%Cr-0.50%Mo creep resisting steels.
Zalety
- Developed for 5%Cr-0.50%Mo creep resisting steels
- Designed for high strength and improved corrosion resistance with hot hydrogen gas, super-heated steam, and Sulphur crude oil
- This weld metal has also been used successfully for subsequent nitriding, for example in the repair of 3Cr- 1Mo-V and 2Cr-Mo-1A1 (BS En40C, En41) steels used for molds for injection-molding of plastics.
Informacje o usługach
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. Strona wyszukiwania kart SDS
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.28 | ER80S-B6 |
MECHANICAL PROPERTIES
Classification | Postweld Heat Treatment | Shielding Gas | Polarity |
Yield Strength @ 0.2% Offset
MPa (ksi) |
Tensile Strength
MPa (ksi) |
Elongation
% |
---|---|---|---|---|---|---|
ER80S-B6 Requirement | 100% Ar | DC- | 470 (68) min. | 550 (80) min. | 17 min. | |
Typical Result, Stress relieved | 1 hour @ 750°C (1380°F) | 100% Ar | DC- | 560 (82) | 670 (97) | 25 |
DEPOSIT COMPOSITION
Classification | Shielding Gas |
---|---|
Typical Result | 100% Ar |
WIRE COMPOSITION
Classification | %C | %Cr | %Mn | %Mo | %Ni | %P | %S | %Si | %Total Cu |
---|---|---|---|---|---|---|---|---|---|
ER80S-B6 Requirement | 0.10 min. | 4.50 - 6.00 | 0.40 - 0.70 | 0.45 - 0.65 | 0.60 max. | 0.025 max. | 0.025 max. | 0.50 min. | 0.35 max. |
Typical Result | 0.08 | 5.66 | 0.48 | 0.56 | 0.10 | 0.010 | 0.008 | 0.40 | 0.10 |