SuperGlaze® 4047 aluminum alloy has a very high silicon content 11-13 % with low melting point for excellent fluidity while welding or brazing.
Özellikleri
- Substitute for 4043 to increase Silicon in weld metal
- Minimize hot cracking to produce higher fillet weld shear strength
- Cosmetic appearing welds
- Lower melting point and higher fluidity than 4043 wires
Servis Bilgileri
Ayrıca İhtiyacınız Olabilir
BEFORE USE, READ AND UNDERSTAND THE SAFETY DATA SHEET (SDS) FOR THIS PRODUCT AND SPECIFIC INFORMATION PRINTED ON THE PRODUCT CONTAINER. SDS Arama sayfası
Test sonucunu görün sorumluluk reddi
CONFORMANCE
CONFORMANCES | SPECIFICATION | CLASSIFICATION |
---|---|---|
AWS | AWS A5.10 | ER4047 |
WIRE COMPOSITION
Classification | %Be | %Mg | %Zn | %Cu | %Fe | %Mn | %Si |
---|---|---|---|---|---|---|---|
ER4047 Requirement | 0.0003 max. | 0.10 max. | 0.20 max. | 0.30 max. | 0.8 max. | 0.15 max. | 11.0 - 13.0 |
Typical Result | 0.0000 | 0.00 | 0.00 | 0.00 | 0.1 | 0.00 | 12.1 |
TYPICAL OPERATING PROCEDURES
Diameter | Shielding Gas |
Gas Flow
L/min (CFH) |
Polarity |
CTWD
mm (in.) |
Wire Feed Speed
m/min (in/min) |
Voltage
volts |
Approx. Current
amps |
---|---|---|---|---|---|---|---|
0.9 mm (.035") | 100% Ar | 14-24 (30-50) | DC+ | 12.7 (¹/₂) - 15.9 (⁵/₈) | 14.9 (585) | 23.3 | 170 |
1.2 mm (3/64") | 100% Ar | 14-24 (30-50) | DC+ | 12.7 (¹/₂) - 15.9 (⁵/₈) | 8.9 (350) | 25.2 | 195 |
1.6 mm (1/16") | 100% Ar | 14-24 (30-50) | DC+ | 12.7 (¹/₂) - 15.9 (⁵/₈) | 6.4 (250) | 24.0 | 240 |